Galvanic corrosion occurs when dissimilar metals contact in electrolyte; more active metal (anode) corrodes preferentially.

Steg-för-steg-guide

  1. 1Input two metals and galvanic series position
  2. 2Calculate galvanic potential
  3. 3Determine which metal corrodes and rate

Lösta exempel

Ingång
Zinc (anode) + steel (cathode) in seawater
Resultat
Zinc sacrificially corrodes, protecting steel (intentional use)

Vanliga misstag att undvika

  • Assuming only one metal corrodes (wrong)
  • Not understanding sacrificial anode concept

Vanliga frågor

How do you prevent galvanic corrosion?

Use same metal, isolate with non-conductive gasket, or apply protective coating.